전체메뉴

Tech University of Korea

High Temperature
Interfacial Property Lab

국외

44

J. Myeong,  J. Park, K. Kim, H. Shibata, Y, Byeun & Y. Chung: "Reaction Mechanism of MgAl2O4 Refractories in Contact with a Liquid Ferromanganese Metal", Metals and Materials International, 2024. DOI :  https://doi.org/10.1007/s12540-024-01820-8 

파일다운로드
43

G.Kim & Y.Chung: "Dissolution Behavior of MgAl2O4 Spinel Inclusions in Mold Slag", Steel research international, Volume 95(7), 2024. DOI :  https://doi.org/10.1002/srin.202400039?

파일다운로드
42

J.Myung & Y.Chung: "Degradation behavior of MgO-C in contact with liquid steel with/without Ar blowing" Metallurgical and Materials Transaction B. Volume 55, pages 83-91, 2024. DOI :  https://doi.org/10.1007/s11663-023-02941-y

 

파일다운로드
41

I.Hwang & Y.Chung: "Physical and Chemical Wetting Behavior Between MgO-C and Liquid Slag With Varying Slag Composition", Metallurgical and Materials Transactions B, Vol. 54, pp.2881-2888. 2023. DOI: https://doi.org/10.1007/s11663-023-02910-5

파일다운로드
40
T.Kwack, H.UM & Y.Chung: "Activation Energy of Alumina Dissolution in FeO-Bearing Slags", Metals 2023, 13(10), 1702. DOI : https://doi.org/10.3390/met13101702
파일다운로드
39

S.Jeon, J.Myung & Y.Chung: "Initial Wetting Phenomena of MgO-SiO2 Liquid Slag on MgO-C Refractories", Metallurgical and Materials Transactions B, Vol. 54(1), pp.34-42. 2022. DOI : https://doi.org/10.1007/s11663-022-02684-2

 

파일다운로드
38

H. Um, S. Yeo, Y. B. Kang & Y. Chung: "The effect of FexO content on dissolution behavior of an alumina inclusion in CaO-Al2O3-SiO2-FexO slag by a single hot thermocouple technique", Ceramics International, Vol. 48(23), pp. 35301-35309. 2022. DOI : https://doi.org/10.1016/j.ceramint.2022.08.132 

파일다운로드
37

S. Lee & Y. Chung: "The effect of C content in MgO-C on dissolution behavior in CaO-SiO2-Al2O3 slag", Ceramics International, Vol. 48(18), pp. 26984-26991, 2022. DOI : https://doi.org/10.1016/j.ceramint.2022.06.010 

파일다운로드
36

C. Yoo, J. Myung & Y. Chung: "Wetting and Spreading Kinetics between Liquid CaO-SiO2 Slags and a Solid SiO2", ISIJ International, Vol. 61(12), pp. 2923-2928, 2021. DOI : https://doi.org/10.2355/isijinternational.ISIJINT-2021-191?

파일다운로드
35

S. Yeo, H. Um & Y. Chung: "The Effect of Alumina Activity on Dissolution Behavior of Alumina Particles in CaO-Al2O3-SiO2 Slags", Metallurgical and Materials Transactions B, Vol. 52(6), pp. 3938-3945, 2021. DOI : https://doi.org/10.1007/s11663-021-02309-0

파일다운로드
34

T. S. Jeong, M. K. Oh, Y. Chung & J. H. Park: "Effect of White Mud Addition on Desulfurization Rate of Molten Steel", Metallurgical and Materials Transactions B, Vol. 52(6), pp. 3596-3605, 2021. DOI : https://doi.org/10.1007/s11663-021-02343-y

파일다운로드
33

J. Lee, J. Myung & Y. Chung: "Degradation Kinetics of MgO-C Refractory at High Temperature", Metallurgical and Materials Transactions B, Vol. 52(3), pp. 1179-1185, 2021. DOI : https://doi.org/10.1007/s11663-021-02106-9 

파일다운로드
32

Y. Kim, Y. Kashiwaya & Y. Chung: "Effect of varying Al2O3 contents of CaO-Al2O3-SiO2 slags on lumped MgO dissolution", Ceramics International, Vol. 46(5), pp. 6205-6211, 2020. DOI : https://doi.org/10.1016/j.ceramint.2019.11.088 

파일다운로드
31

J. S. Han, Y. Chung & J. H. Park: "Influence of exposure temperature on degradation of magnesia refractory by steel refining slags", Metals and Materials International, Vol. 25(5), pp. 1360-1365, 2019. DOI : https://doi.org/10.1007/s12540-019-00286-3 

파일다운로드
30

J. H. Heo, J. S. Yoo, Y. Chung & J. H. Park: "Influence of Aluminum-Carbon Composite Pellets on FeO Reduction and Iron Recovery from Electric Arc Furnace Slag", Metallurgical and Materials Transactions B, Vol. 50(2), pp. 903-913, 2019. DOI : https://doi.org/10.1007/s11663-018-1484-4 

파일다운로드
29

H. S. Park, Y. Kim, S. Kim, T. Yoon, Y. Kim & Chung: "A study on the wetting behavior of liquid iron on forsterite, mullite, spinel and quasi-corundum substrates", Ceramics International, Vol. 44(15), pp. 17585-17591, 2018. DOI : https://doi.org/10.1016/j.ceramint.2018.05.226 

파일다운로드
28

J. S. Han, J. G. Kang, J. H. Shin, Y. Chung & J. H. Park: "Influence of CaF2 in calcium aluminate-based slag on the degradation of magnesia refractory", Ceramics International, Vol. 44(11), pp. 13197-13204, 2018. DOI : https://doi.org/10.1016/j.ceramint.2018.04.145 

파일다운로드
27

J. Jeon, Y. Kang, J. H. Park & Y. Chung: "Corrosion-erosion behavior of MgAl2O4 spinel refractory in contact with high MnO slag", Ceramics International, Vol. 43(17), pp. 15074-15079, 2017. DOI : https://doi.org/10.1016/j.ceramint.2017.08.034 

파일다운로드
26

T. Yoon, K. Lee, B. Lee & Y. Chung: "Wetting, spreading and penetration phenomena of slags on MgAl2O4 spinel refractories", ISIJ International, Vol. 57(8), pp. 1327-1333, 2017. DOI : https://doi.org/10.2355/isijinternational.ISIJINT-2016-578 

파일다운로드
25

T. S. Kim, Y. Chung, L. Holappa & J. H. Park: "Effect of rice husk ash insulation powder on the reoxidation behavior of molten steel in continuous casting tundish", Metallurgical and Materials Transactions B, Vol. 48(3), pp. 1736-1747, 2017. DOI : https://doi.org/10.1007/s11663-017-0971-3 

파일다운로드